| ABSTRACT |
Banana fiber reinforced with graphite offers a greener path for blast protection, yet its full capacity remains unclear. Conventional bomb blankets rely on heavy, non-degradable synthetic fabrics, driving the search for lighter and sustainable alternatives. This work aims to identify the optimum combination of chemical treatment, graphite loading, and weave pattern for banana fiber/epoxy composites intended for blast mitigation applications. Banana fibers extracted from pseudostems were woven into plain, twill, and satin architectures and chemically treated using sulfuric acid hydrolysis, followed by composite fabrication with 0.5 wt.% commercial graphite powder using the selected most efficient treatment. Tensile testing using a Universal Testing Machine (UTM) showed that the composite treated with 1% sulfuric acid achieved the highest ultimate tensile strength of 5.011 MPa and a strain at break of 5.135%, indicating effective stress transfer due to controlled removal of amorphous fiber components. Impact resistance measured using an Izod Impact Tester demonstrated that the twill weave configuration provided the highest impact energy absorption of approximately 4.7 J, attributed to improved yarn interlocking and stress redistribution. Water absorption testing revealed that the graphite-enhanced composite treated with 1% sulfuric acid exhibited the lowest moisture uptake after prolonged immersion, indicating improved resistance to moisture ingress. X-ray Diffraction (XRD) analysis, suggests the presence of graphite within the composite through a characteristic diffraction peak at approximately 2θ ≈ 26.4°, corresponding to the (002) plane of graphite, along with intensified cellulose crystalline peaks around 2θ ≈ 22°, indicating increased fiber crystallinity after acid treatment. Fourier Transform Infrared Spectroscopy (FTIR) analysis, indicates characteristic O¿H stretching bands in the range of 3200¿3600 cm⁻¹ associated with cellulose, reduced C=O peaks near 1730 cm⁻¹ corresponding to hemicellulose removal after sulfuric acid treatment, and prominent C¿O¿C and C¿H vibrations attributed to the epoxy matrix, confirming fiber¿matrix compatibility.OM observations confirmed experimentally that fibers treated with 1% sulfuric acid exhibited clean and continuous surfaces with minimal damage, while corresponding SEM features support the observed morphology. Small-scale blast testing further confirmed that the graphite-enhanced banana fiber composite treated with 1% sulfuric acid and configured in a twill weave remained structurally intact after explosive loading, with damage localized near the impact region. In conclusion, the study establishes that a banana fiber/epoxy composite treated with 1% sulfuric acid, reinforced with low graphite content, and arranged in a twill weave offers a promising lightweight and biodegradable alternative for blast protection applications.
|